MISE EN EVIDENCE DE DEFAUTS ACTIFS LUMINESCENTS DANS LE ZnO PAR PHOTOLUMINESCENCE ET TSC

dc.contributor.authorChabane, L.
dc.contributor.authorZebbar, N.
dc.contributor.authorZaaboub, Z.
dc.contributor.authorTata, S.
dc.contributor.authorKechouane, M.
dc.date.accessioned2019-06-02T10:29:13Z
dc.date.available2019-06-02T10:29:13Z
dc.date.issued2018-02-05
dc.descriptionSéminaire National Sur Laser Solaire Et Matériaux ElOeued 5-6 Février 2018en_US
dc.description.abstractIn this work, we have, experimentally, investigated the luminescence defect in ZnO thin film deposited onto crystalline Si substrate. The studied film was deposited by DC reactive sputtering technique, under (Ar + O2) plasma at 373 K, durig 1 hour and annealed at 573 K during 1 hour. The UV-Visible transmittance and ellipsometrie characterisations revealed that the optical energy band gap and the film thickness are respectively, around to 3.35 eV and 50 nm. The photoluminescence spectrum measured at room temperature indicates that the deposited film presente a UV luminescence peak at 384 nm (3.21 eV). The current-potentialtemperature and the stimulated current measurements indicate the presence of a shallow level with activation energy around to 0.35 eV, attributed to the interstial zinc or oxygen vacancies.en_US
dc.identifier.urihttps://dspace.univ-eloued.dz/handle/123456789/2416
dc.language.isofren_US
dc.publisherUniversity of Eloued جامعة الواديen_US
dc.subjectZinc oxide, thin films, photolumencence, TSC measurments, reacctive sputtering.en_US
dc.titleMISE EN EVIDENCE DE DEFAUTS ACTIFS LUMINESCENTS DANS LE ZnO PAR PHOTOLUMINESCENCE ET TSCen_US
dc.typeOtheren_US

Files

Original bundle

Now showing 1 - 1 of 1
No Thumbnail Available
Name:
MISE EN EVIDENCE DE DEFAUTS ACTIFS LUMINESCENTS.pdf
Size:
398.8 KB
Format:
Adobe Portable Document Format
Description:
Séminaire National Sur Laser Solaire Et Matériaux ElOeued 5-6 Février 2018

License bundle

Now showing 1 - 1 of 1
No Thumbnail Available
Name:
license.txt
Size:
1.71 KB
Format:
Item-specific license agreed upon to submission
Description: